Fig. 7 | Journal of Nanobiotechnology

Fig. 7

From: Accelerated full-thickness skin wound tissue regeneration by self-crosslinked chitosan hydrogel films reinforced by oxidized CNC-AgNPs stabilized Pickering emulsion for quercetin delivery

Fig. 7

Characterization of CS-PE films with varying glycerol content (A) Representative photographs and SEM images (surface and cross-section) (3 kV, x500, and scale bar 10 µM) (B) Porosity (C) Swelling ratio (D) Water vapour transmission rate and (E) Dressing pH. Values were expressed as mean ± SD, **P < 0.01, ***P < 0.001 vs. CS-PE-2.5% Gly